‹ 全部性质

Magnetic properties

Dia-, para-, ferro- and other magnetic behavior of the elemental substance, with Curie/Néel temperatures where applicable. reference: 298.15 K (25 °C), 1 bar.

可用数据 95 / 118 反铁磁性 1抗磁性 34铁磁性 3顺磁性 57 无数据 23
T_C 最小值 -259.15 °C Samarium
T_C 最大值 1114.85 °C Cobalt
T_N 最小值 -253.25 °C Neodymium
T_N 最大值 37.85 °C Chromium

显示 118 / 118 个元素

符号名称显示详情
1HHydrogen抗磁性 H₂ (molecule) 气态 298.15 K(25 °C),1 bar — — — 实测值
2HeHelium抗磁性 He (atom) 气态 298.15 K(25 °C),1 bar — — — 实测值
3LiLithium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
4BeBeryllium抗磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
5BBoron抗磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
6CCarbon抗磁性 graphite 固态 298.15 K(25 °C),1 bar — — — 实测值
7NNitrogen抗磁性 N₂ (molecule) 气态 298.15 K(25 °C),1 bar — — — 实测值
8OOxygen顺磁性 O₂ (molecule) 气态 298.15 K(25 °C),1 bar — -249.35 -249.3 °C23.8 K (-249.3 °C): 反铁磁 → 顺磁 — Solid α-O₂ orders antiferromagnetically; the transition coincides with the α→β structural transition. 实测值
9FFluorine抗磁性 F₂ (molecule) 气态 298.15 K(25 °C),1 bar — — — 实测值
10NeNeon抗磁性 Ne (atom) 气态 298.15 K(25 °C),1 bar — — — 实测值
11NaSodium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
12MgMagnesium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
13AlAluminum顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
14SiSilicon抗磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
15PPhosphorus抗磁性 white phosphorus P₄ (standard state) 固态 298.15 K(25 °C),1 bar — — — 实测值
16SSulfur抗磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
17ClChlorine抗磁性 Cl₂ (molecule) 气态 298.15 K(25 °C),1 bar — — — 实测值
18ArArgon抗磁性 Ar (atom) 气态 298.15 K(25 °C),1 bar — — — 实测值
19KPotassium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
20CaCalcium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
21ScScandium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
22TiTitanium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
23VVanadium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
24CrChromium反铁磁性 — 固态 298.15 K(25 °C),1 bar — 37.85 37.9 °C311 K (37.9 °C): 反铁磁 → 顺磁 实测值
25MnManganese顺磁性 α-Mn (complex cubic) 固态 298.15 K(25 °C),1 bar — -178.15 -178.1 °C95 K (-178.1 °C): 反铁磁 → 顺磁 — Complex order of α-Mn with several inequivalent Mn sites. 实测值
26FeIron铁磁性 α-Fe (bcc) 固态 298.15 K(25 °C),1 bar 769.85 769.9 °C— 1043 K (769.9 °C): 铁磁 → 顺磁 实测值
27CoCobalt铁磁性 α-Co (hcp) 固态 298.15 K(25 °C),1 bar 1114.85 1,114.9 °C— 1388 K (1,114.9 °C): 铁磁 → 顺磁 实测值
28NiNickel铁磁性 — 固态 298.15 K(25 °C),1 bar 353.85 353.9 °C— 627 K (353.9 °C): 铁磁 → 顺磁 实测值
29CuCopper抗磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
30ZnZinc抗磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
31GaGallium抗磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
32GeGermanium抗磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
33AsArsenic抗磁性 gray arsenic 固态 298.15 K(25 °C),1 bar — — — 实测值
34SeSelenium抗磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
35BrBromine抗磁性 Br₂ (molecule) 液态 298.15 K(25 °C),1 bar — — — 实测值
36KrKrypton抗磁性 Kr (atom) 气态 298.15 K(25 °C),1 bar — — — 实测值
37RbRubidium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
38SrStrontium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
39YYttrium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
40ZrZirconium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
41NbNiobium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
42MoMolybdenum顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
43TcTechnetium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
44RuRuthenium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
45RhRhodium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
46PdPalladium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
47AgSilver抗磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
48CdCadmium抗磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
49InIndium抗磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
50SnTin顺磁性 β-Sn (white tin) 固态 298.15 K(25 °C),1 bar — — — 实测值
51SbAntimony抗磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
52TeTellurium抗磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
53IIodine抗磁性 I₂ (molecule) 固态 298.15 K(25 °C),1 bar — — — 实测值
54XeXenon抗磁性 Xe (atom) 气态 298.15 K(25 °C),1 bar — — — 实测值
55CsCesium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
56BaBarium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
57LaLanthanum顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
58CeCerium顺磁性 γ-Ce (fcc) 固态 298.15 K(25 °C),1 bar — — — 实测值
59PrPraseodymium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
60NdNeodymium顺磁性 — 固态 287.7 K (14.6 °C), 1 bar — -253.25 -253.2 °C19.9 K (-253.2 °C): 反铁磁 → 顺磁 — Several magnetic phases below 20 K. 实测值
61PmPromethium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
62SmSamarium顺磁性 — 固态 291 K (17.9 °C), 1 bar -259.15 -259.1 °C-167.15 -167.1 °C14 K (-259.1 °C): 锥形铁磁 → 反铁磁 • 106 K (-167.1 °C): 反铁磁 → 顺磁 — Sources give 105–110 K for the Néel point. 实测值
63EuEuropium顺磁性 — 固态 298.15 K(25 °C),1 bar — -182.75 -182.7 °C90.4 K (-182.7 °C): 螺旋反铁磁 → 顺磁 实测值
64GdGadolinium顺磁性 — 固态 300 K (27 °C), 1 bar 20.25 20.3 °C— 293.4 K (20.3 °C): 铁磁 → 顺磁 实测值
65TbTerbium顺磁性 — 固态 300 K (27 °C), 1 bar -54.15 -54.1 °C-43.15 -43.1 °C219 K (-54.1 °C): 铁磁 → 螺旋反铁磁 • 230 K (-43.1 °C): 螺旋反铁磁 → 顺磁 实测值
66DyDysprosium顺磁性 — 固态 293 K (20 °C), 1 bar -185.15 -185.1 °C-94.15 -94.1 °C88 K (-185.1 °C): 铁磁 → 螺旋反铁磁 — Coupled with a first-order structural transition. • 179 K (-94.1 °C): 螺旋反铁磁 → 顺磁 实测值
67HoHolmium顺磁性 — 固态 300 K (27 °C), 1 bar -253.15 -253.1 °C-141.15 -141.1 °C20 K (-253.1 °C): 锥形铁磁 → 螺旋反铁磁 • 132 K (-141.1 °C): 螺旋反铁磁 → 顺磁 实测值
68ErErbium顺磁性 — 固态 300 K (27 °C), 1 bar -254.15 -254.1 °C-189.15 -189.1 °C19 K (-254.1 °C): 锥形铁磁 → 反铁磁 • 52 K (-221.1 °C): Reorganization of the antiferromagnetic structure. • 84 K (-189.1 °C): 反铁磁 → 顺磁 实测值
69TmThulium顺磁性 — 固态 300 K (27 °C), 1 bar -241.15 -241.1 °C-217.15 -217.1 °C32 K (-241.1 °C): 铁磁 → 反铁磁 • 56 K (-217.1 °C): 反铁磁 → 顺磁 实测值
70YbYtterbium顺磁性 β-Yb 固态 298.15 K(25 °C),1 bar — — — 实测值
71LuLutetium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
72HfHafnium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
73TaTantalum顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
74WTungsten顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
75ReRhenium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
76OsOsmium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
77IrIridium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
78PtPlatinum顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
79AuGold抗磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
80HgMercury抗磁性 — 液态 298.15 K(25 °C),1 bar — — — 实测值
81TlThallium抗磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
82PbLead抗磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
83BiBismuth抗磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
84PoPolonium— — 固态 — — — — —
85AtAstatine— — 固态 — — — — —
86RnRadon抗磁性 预测 Rn (atom) 气态 298.15 K(25 °C),1 bar — — — 预测值
87FrFrancium顺磁性 预测 — 固态 298.15 K(25 °C),1 bar — — — 预测值
88RaRadium— — 固态 — — — — —
89AcActinium— — 固态 — — — — —
90ThThorium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
91PaProtactinium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
92UUranium顺磁性 α-U (orthorhombic) 固态 298.15 K(25 °C),1 bar — — — 实测值
93NpNeptunium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
94PuPlutonium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
95AmAmericium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
96CmCurium顺磁性 — 固态 298.15 K(25 °C),1 bar — -221.15 -221.1 °C52 K (-221.1 °C): 反铁磁 → 顺磁 — α-Cm; the β form shows a ferrimagnetic transition near 205 K. 实测值
97BkBerkelium顺磁性 — 固态 298.15 K(25 °C),1 bar — -239.15 -239.1 °C34 K (-239.1 °C): 反铁磁 → 顺磁 实测值
98CfCalifornium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
99EsEinsteinium顺磁性 — 固态 298.15 K(25 °C),1 bar — — — 实测值
100FmFermium— — 固态 — — — — —
101MdMendelevium— — 固态 — — — — —
102NoNobelium— — 固态 — — — — —
103LrLawrencium— — 固态 — — — — —
104RfRutherfordium— — 固态 — — — — —
105DbDubnium— — — — — — — —
106SgSeaborgium— — — — — — — —
107BhBohrium— — — — — — — —
108HsHassium— — — — — — — —
109MtMeitnerium— — — — — — — —
110DsDarmstadtium— — — — — — — —
111RgRoentgenium— — — — — — — —
112CnCopernicium— — 气态 — — — — —
113NhNihonium— — 固态 — — — — —
114FlFlerovium— — 气态 — — — — —
115McMoscovium— — 固态 — — — — —
116LvLivermorium— — 固态 — — — — —
117TsTennessine— — 固态 — — — — —
118OgOganesson— — 气态 — — — — —

来源与备注

  • The primary record uses one explicitly named form of the simple substance per element; other allotropic forms and states of aggregation are shown in the row expansion and are never mixed with the primary data.
  • Curie temperatures T_C and Néel temperatures T_N are shown for every element with a known transition — including those already above their ordering temperature at 25 °C. T_C and T_N are counted separately in the summary.
  • Magnetic properties of compounds or isolated atoms are never transferred to the simple substance.
  • Superconductivity is shown separately (with its own critical temperature, which is never presented as a Curie temperature).
  • Volume magnetic susceptibility χ (SI, dimensionless) is given in the row expansion with its measurement conditions; for nonlinear responses (ferromagnets) it is not a universal constant.